People | Locations | Statistics |
---|---|---|
Naji, M. |
| |
Motta, Antonella |
| |
Aletan, Dirar |
| |
Mohamed, Tarek |
| |
Ertürk, Emre |
| |
Taccardi, Nicola |
| |
Kononenko, Denys |
| |
Petrov, R. H. | Madrid |
|
Alshaaer, Mazen | Brussels |
|
Bih, L. |
| |
Casati, R. |
| |
Muller, Hermance |
| |
Kočí, Jan | Prague |
|
Šuljagić, Marija |
| |
Kalteremidou, Kalliopi-Artemi | Brussels |
|
Azam, Siraj |
| |
Ospanova, Alyiya |
| |
Blanpain, Bart |
| |
Ali, M. A. |
| |
Popa, V. |
| |
Rančić, M. |
| |
Ollier, Nadège |
| |
Azevedo, Nuno Monteiro |
| |
Landes, Michael |
| |
Rignanese, Gian-Marco |
|
Vienna, John D.
in Cooperation with on an Cooperation-Score of 37%
Topics
Publications (6/6 displayed)
- 2024Insights on the structure and properties of sodium iron phosphate glasses from molecular dynamics simulationscitations
- 2020Near-field corrosion interactions between glass and corrosion resistant alloyscitations
- 2020Tomographic mapping of the nanoscale water-filled pore structure in corroded borosilicate glasscitations
- 2018Impacts of glass composition, pH, and temperature on glass forward dissolution ratecitations
- 2017Glass Transition Temperature- and Specific Volume- Composition Models for Tellurite Glasses
- 2006Corrosion of low level vitrified radioactive waste in a loamy soil
Places of action
Organizations | Location | People |
---|
article
Corrosion of low level vitrified radioactive waste in a loamy soil
Abstract
Corrosion of high sodium borosilicate glass K-26 was examined over 16 years of storage in a loamy soil. An altered layer was formed on the glass surface which is inhomogeneous in thickness and composition. This layer is mostly amorphous with small crystalline inclusions. The pH of the groundwater in contact with the radioactive glass gradually from 7·5 to 7·9 and the groundwater was slightly contaminated with 137Cs at levels from ~20 to below 10 Bq/L after 16 years. The corrosion rate of glass diminishes with time and is 0·22 µg/cm2 day after 16 years.