People | Locations | Statistics |
---|---|---|
Naji, M. |
| |
Motta, Antonella |
| |
Aletan, Dirar |
| |
Mohamed, Tarek |
| |
Ertürk, Emre |
| |
Taccardi, Nicola |
| |
Kononenko, Denys |
| |
Petrov, R. H. | Madrid |
|
Alshaaer, Mazen | Brussels |
|
Bih, L. |
| |
Casati, R. |
| |
Muller, Hermance |
| |
Kočí, Jan | Prague |
|
Šuljagić, Marija |
| |
Kalteremidou, Kalliopi-Artemi | Brussels |
|
Azam, Siraj |
| |
Ospanova, Alyiya |
| |
Blanpain, Bart |
| |
Ali, M. A. |
| |
Popa, V. |
| |
Rančić, M. |
| |
Ollier, Nadège |
| |
Azevedo, Nuno Monteiro |
| |
Landes, Michael |
| |
Rignanese, Gian-Marco |
|
Hadasik, E.
in Cooperation with on an Cooperation-Score of 37%
Topics
Publications (4/4 displayed)
- 2017Kinetics of static recrystallization in the coarse-grained Fe-40 at.%Al-Zr-B alloycitations
- 2015Optimization of laboratory hot rolling of brittle Fe-40at.%Al-Zr-B aluminidecitations
- 2014Plasticity and microstructure of magnesium – lithium alloyscitations
- 2013Forecasting of Corrosion Properties of Steel Wires for Production of Guide Wires for Cardiological Treatmentcitations
Places of action
Organizations | Location | People |
---|
article
Plasticity and microstructure of magnesium – lithium alloys
Abstract
The article presents the results of tests connected with influence of strain parameters on the susceptibility to hot working of magnesium lithium alloys with lithium content of 7.5% mass. Plasticity tests were conducted in compression test from room temperature up to 400°C with strain rate of 0.1s-1. Conducted tests allowed for determination of susceptibility of magnesium alloys with different lithium content to hot working. The results were compared with typical alloy AZ31. The results of influence of deformation temperature on the microstructure of tested alloys are also presented in this paper.