People | Locations | Statistics |
---|---|---|
Naji, M. |
| |
Motta, Antonella |
| |
Aletan, Dirar |
| |
Mohamed, Tarek |
| |
Ertürk, Emre |
| |
Taccardi, Nicola |
| |
Kononenko, Denys |
| |
Petrov, R. H. | Madrid |
|
Alshaaer, Mazen | Brussels |
|
Bih, L. |
| |
Casati, R. |
| |
Muller, Hermance |
| |
Kočí, Jan | Prague |
|
Šuljagić, Marija |
| |
Kalteremidou, Kalliopi-Artemi | Brussels |
|
Azam, Siraj |
| |
Ospanova, Alyiya |
| |
Blanpain, Bart |
| |
Ali, M. A. |
| |
Popa, V. |
| |
Rančić, M. |
| |
Ollier, Nadège |
| |
Azevedo, Nuno Monteiro |
| |
Landes, Michael |
| |
Rignanese, Gian-Marco |
|
Cocić, Mira
University of Belgrade
in Cooperation with on an Cooperation-Score of 37%
Topics
Publications (4/4 displayed)
- 2022Characterization of material sintered from the final flotation waste and zeolitic tuffcitations
- 2017Application of the final flotation waste for obtaining the glass-ceramic materialscitations
- 2017Application of the final flotation waste for obtaining the glass-ceramic materialscitations
- 2016Final flotation waste kinetics of sintering at different heating regimescitations
Places of action
Organizations | Location | People |
---|
article
Final flotation waste kinetics of sintering at different heating regimes
Abstract
<jats:p>In the copper extraction, especially during the process of flotationenrichment and the pyrometallurgical processing, the waste materials thatrepresent huge polluters of environment are being generated. In order toexamine the application of Final flotation waste (FFW) in the manufacturingof new materials from the glass-ceramic group phase and mineral compositionwere examined as well as thermal properties. FFW kinetics of sintering hasbeen tested at different dyamics (1?C/min, 29?C/min and 43?C/min), in orderto find the optimum conditions for sintering with a minimum amount of energyand time consumption. The samples were examined using: X-ray diffraction,X-ray fluorescence analysis, SEM (Scanning Electron Microscopy) and thermalmicroscopy. The best results for the production of glass ceramic materialswere obtained during the sintering at heating regime of 29?C/min.</jats:p>