People | Locations | Statistics |
---|---|---|
Naji, M. |
| |
Motta, Antonella |
| |
Aletan, Dirar |
| |
Mohamed, Tarek |
| |
Ertürk, Emre |
| |
Taccardi, Nicola |
| |
Kononenko, Denys |
| |
Petrov, R. H. | Madrid |
|
Alshaaer, Mazen | Brussels |
|
Bih, L. |
| |
Casati, R. |
| |
Muller, Hermance |
| |
Kočí, Jan | Prague |
|
Šuljagić, Marija |
| |
Kalteremidou, Kalliopi-Artemi | Brussels |
|
Azam, Siraj |
| |
Ospanova, Alyiya |
| |
Blanpain, Bart |
| |
Ali, M. A. |
| |
Popa, V. |
| |
Rančić, M. |
| |
Ollier, Nadège |
| |
Azevedo, Nuno Monteiro |
| |
Landes, Michael |
| |
Rignanese, Gian-Marco |
|
Ebrahimzadeh, Iman
in Cooperation with on an Cooperation-Score of 37%
Topics
Publications (1/1 displayed)
Places of action
Organizations | Location | People |
---|
article
THE EFFECT OF ALUMINA NANOPARTICLES ADDITION ON HIGH-TEMPERATURE WEAR BEHAVIOR OF INTERMETALLIC IRON ALUMINIDE PRODUCED BY THE SPARK PLASMA SINTERING PROCESS
Abstract
<jats:p> The pure iron and aluminum powders were milled with 3[Formula: see text]wt.% and 7[Formula: see text]wt.% of alumina nanoparticles in planetary ball mill in order to produce iron aluminide by mechanical alloying technique. The resulting powder mixture was sintered after the formation of iron aluminide by spark plasma sintering (SPS) method to achieve specimens with the highest densification. SPS technique was utilized on specimens under the condition of 40[Formula: see text]MPa pressure at 950<jats:sup>∘</jats:sup>C for 5[Formula: see text]min. The microstructures were analyzed after sintering using scanning electron microscopy and EDS analysis. The results indicated that the aluminide iron phase has been produced at high purity. The sintered specimens were treated under hardness and density tests, and it was characterized that the specimen included 3[Formula: see text]wt.% of alumina nanoparticles had the highest microhardness. Likewise, it was revealed that the unreinforced sample had a maximum relative density. The wear behavior of specimens was performed at 600<jats:sup>∘</jats:sup>C. The results of weight loss showed after 1000[Formula: see text]m of wear test, the weight loss of unreinforced specimen was reduced up to 0.21[Formula: see text]g while the specimen with 3[Formula: see text]wt.% of alumina nanoparticle indicated the lowest weight loss about 0.02[Formula: see text]g. The worn surfaces were evaluated by scanning electron microscopy which indicated that the main wear mechanism at high temperature included adhesive wear and delamination. </jats:p>