People | Locations | Statistics |
---|---|---|
Naji, M. |
| |
Motta, Antonella |
| |
Aletan, Dirar |
| |
Mohamed, Tarek |
| |
Ertürk, Emre |
| |
Taccardi, Nicola |
| |
Kononenko, Denys |
| |
Petrov, R. H. | Madrid |
|
Alshaaer, Mazen | Brussels |
|
Bih, L. |
| |
Casati, R. |
| |
Muller, Hermance |
| |
Kočí, Jan | Prague |
|
Šuljagić, Marija |
| |
Kalteremidou, Kalliopi-Artemi | Brussels |
|
Azam, Siraj |
| |
Ospanova, Alyiya |
| |
Blanpain, Bart |
| |
Ali, M. A. |
| |
Popa, V. |
| |
Rančić, M. |
| |
Ollier, Nadège |
| |
Azevedo, Nuno Monteiro |
| |
Landes, Michael |
| |
Rignanese, Gian-Marco |
|
Chrzanowski, Wojciech
in Cooperation with on an Cooperation-Score of 37%
Topics
Publications (8/8 displayed)
- 2014Bioactive nanocomposite PLDL/nano-hydroxyapatite electrospun membranes for bone tissue engineeringcitations
- 2010Tailoring Cell Behavior on Polymers by the Incorporation of Titanium Doped Phosphate Glass Fillercitations
- 2010<i>In vitro</i> studies on the influence of surface modification of Ni–Ti alloy on human bone cellscitations
- 2009Structure and properties of strontium-doped phosphate-based glassescitations
- 2009Incorporation of vitamin E in poly(3hydroxybutyrate)/Bioglass composite films: effect on surface properties and cell attachment.citations
- 2009Doping of a high calcium oxide metaphosphate glass with titanium dioxidecitations
- 2008Nanomechanical evaluation of nickel–titanium surface properties after alkali and electrochemical treatmentscitations
- 2008Chemical, Corrosion and Topographical Analysis of Stainless Steel Implants after Different Implantation Periodscitations
Places of action
Organizations | Location | People |
---|
article
Nanomechanical evaluation of nickel–titanium surface properties after alkali and electrochemical treatments
Abstract
<jats:p>In this paper, the suitability of alkali treatment followed by heat treatment at 600°C, and spark oxidation for nickel–titanium, intended for medical applications such as pins, wires and clamps, was evaluated on the basis of nanomechanical and wear testing. In addition, the chemical composition and topography of the surface layer, wetting ability, corrosion resistance and influence of the heat treatment on structure of the alloy were also investigated. The results showed that the highest hardness was observed for alkali-treated samples, and this could be correlated with the structure of the sample that contained martensite and a higher phase transformation temperature. This treatment caused a very large increase of nickel in the top layer and decreased resistance in pitting corrosion. These results disqualified the treatment to be considered as useful for medical applications. On the other hand, the hardness of the oxidized samples was at the same level as that obtained for ground reference samples. Moreover, the oxide layer was enriched with phosphorus, and it was predominantly composed of TiO<jats:sub>2</jats:sub>and phosphorus oxides. This 3.1 μm thick layer had good adhesion to the substrate as indicated by scratch testing and wear resistant in nanowear testing. However, the oxidation did not significantly increase the corrosion resistance of the alloy compared with reference samples.</jats:p>