People | Locations | Statistics |
---|---|---|
Naji, M. |
| |
Motta, Antonella |
| |
Aletan, Dirar |
| |
Mohamed, Tarek |
| |
Ertürk, Emre |
| |
Taccardi, Nicola |
| |
Kononenko, Denys |
| |
Petrov, R. H. | Madrid |
|
Alshaaer, Mazen | Brussels |
|
Bih, L. |
| |
Casati, R. |
| |
Muller, Hermance |
| |
Kočí, Jan | Prague |
|
Šuljagić, Marija |
| |
Kalteremidou, Kalliopi-Artemi | Brussels |
|
Azam, Siraj |
| |
Ospanova, Alyiya |
| |
Blanpain, Bart |
| |
Ali, M. A. |
| |
Popa, V. |
| |
Rančić, M. |
| |
Ollier, Nadège |
| |
Azevedo, Nuno Monteiro |
| |
Landes, Michael |
| |
Rignanese, Gian-Marco |
|
Mattelaer, Felix
in Cooperation with on an Cooperation-Score of 37%
Topics
Publications (4/4 displayed)
- 2020Thermal and plasma-enhanced atomic layer deposition of yttrium oxide films and the properties of water wettabilitycitations
- 2019Atomic layer deposition of thin films as model electrodes : a case study of the synergistic effect in Fe2O3-SnO2citations
- 2016Novel method for conformal LiMn2O4 thin films fabrication on planar and 3D microstructure substrates
- 2016Manganese oxide films with controlled oxidation state for water splitting devices through a combination of atomic layer deposition and post-deposition annealingcitations
Places of action
Organizations | Location | People |
---|
article
Thermal and plasma-enhanced atomic layer deposition of yttrium oxide films and the properties of water wettability
Abstract
The atomic layer deposition (ALD) of yttrium oxide (Y2O3) is investigated using the liquid precursor Y(EtCp)2(iPr-amd) as the yttrium source with thermal (H2O) and plasma-enhanced (H2O plasma and O2 plasma) processes, respectively. Saturation is confirmed for the growth of the Y2O3 films with each investigated reactant with a similar ALD window from 150 to 300 °C, albeit with a different growth rate. All of the as-deposited Y2O3 films are pure and smooth and have a polycrystalline cubic structure. The as-deposited Y2O3 films are hydrophobic with water contact angles >90°. The water contact angle gradually increased and the surface free energy gradually decreased as the film thickness increased, reaching a saturated value at a Y2O3 film thickness of ∼20 nm. The hydrophobicity was retained during post-ALD annealed at 500 °C in static air for 2 h. Exposure to polar and nonpolar solvents influences the Y2O3 water contact angle. The reported ALD process for Y2O3 films may find potential applications in the field of hydrophobic coatings.