People | Locations | Statistics |
---|---|---|
Naji, M. |
| |
Motta, Antonella |
| |
Aletan, Dirar |
| |
Mohamed, Tarek |
| |
Ertürk, Emre |
| |
Taccardi, Nicola |
| |
Kononenko, Denys |
| |
Petrov, R. H. | Madrid |
|
Alshaaer, Mazen | Brussels |
|
Bih, L. |
| |
Casati, R. |
| |
Muller, Hermance |
| |
Kočí, Jan | Prague |
|
Šuljagić, Marija |
| |
Kalteremidou, Kalliopi-Artemi | Brussels |
|
Azam, Siraj |
| |
Ospanova, Alyiya |
| |
Blanpain, Bart |
| |
Ali, M. A. |
| |
Popa, V. |
| |
Rančić, M. |
| |
Ollier, Nadège |
| |
Azevedo, Nuno Monteiro |
| |
Landes, Michael |
| |
Rignanese, Gian-Marco |
|
Boréave, A.
in Cooperation with on an Cooperation-Score of 37%
Topics
Publications (2/2 displayed)
Places of action
Organizations | Location | People |
---|
article
Isothermal catalytic oxidation of diesel soot on Yttria-stabilized Zirconia
Abstract
Long-term isothermal experiments of soot combustion were performed on Yttria-stabilized Zirconia, an oxygen ionic conductor, at 370,390 and 410 degrees C. At these temperatures, isotopic experiment confirms that mobile YSZ bulk oxygens oxidize soot at the soot/YSZ interface. In parallel, the surface oxygen exchange process replenishes YSZ oxygen atoms. After long-term isothermal experiments, HR-TEM observations reveal that the remaining soot particles form a continuous thin film on some YSZ grains, which inhibits the oxygen potential gradient, then stopping the oxidation process. All these experiments are in good agreement with the proposed fuel-cell type mechanism of soot on YSZ.