People | Locations | Statistics |
---|---|---|
Naji, M. |
| |
Motta, Antonella |
| |
Aletan, Dirar |
| |
Mohamed, Tarek |
| |
Ertürk, Emre |
| |
Taccardi, Nicola |
| |
Kononenko, Denys |
| |
Petrov, R. H. | Madrid |
|
Alshaaer, Mazen | Brussels |
|
Bih, L. |
| |
Casati, R. |
| |
Muller, Hermance |
| |
Kočí, Jan | Prague |
|
Šuljagić, Marija |
| |
Kalteremidou, Kalliopi-Artemi | Brussels |
|
Azam, Siraj |
| |
Ospanova, Alyiya |
| |
Blanpain, Bart |
| |
Ali, M. A. |
| |
Popa, V. |
| |
Rančić, M. |
| |
Ollier, Nadège |
| |
Azevedo, Nuno Monteiro |
| |
Landes, Michael |
| |
Rignanese, Gian-Marco |
|
V., Lalitha K.
in Cooperation with on an Cooperation-Score of 37%
Topics
Publications (1/1 displayed)
Places of action
Organizations | Location | People |
---|
article
Mechanical versus electromechanical hardening in relaxor ferroelectric Na1/2Bi1/2TiO3-BaTiO3 with ZnO inclusions
Abstract
<p>The stress-strain response of composites constituting relaxor 0.94Na<sub>1/2</sub>Bi<sub>1/2</sub>TiO<sub>3</sub>–0.06BaTiO<sub>3</sub> matrix phase with ZnO inclusions is investigated. The ZnO inclusions are found to increase the transformation stress (unpoled) for the relaxor-ferroelectric transformation and the coercive stress (poled) for domain switching. The plastic and remanent strain decreases with increasing volume fraction of the hard ZnO inclusions. This mechanical hardening mechanism is contrasted quantitatively to electromechanical hardening by comparing the transformation stress and coercive stress to the poling field and coercive field respectively, as well as the corresponding plastic strain from mechanical loading to the total strain quantified by electric field loading.</p>