People | Locations | Statistics |
---|---|---|
Naji, M. |
| |
Motta, Antonella |
| |
Aletan, Dirar |
| |
Mohamed, Tarek |
| |
Ertürk, Emre |
| |
Taccardi, Nicola |
| |
Kononenko, Denys |
| |
Petrov, R. H. | Madrid |
|
Alshaaer, Mazen | Brussels |
|
Bih, L. |
| |
Casati, R. |
| |
Muller, Hermance |
| |
Kočí, Jan | Prague |
|
Šuljagić, Marija |
| |
Kalteremidou, Kalliopi-Artemi | Brussels |
|
Azam, Siraj |
| |
Ospanova, Alyiya |
| |
Blanpain, Bart |
| |
Ali, M. A. |
| |
Popa, V. |
| |
Rančić, M. |
| |
Ollier, Nadège |
| |
Azevedo, Nuno Monteiro |
| |
Landes, Michael |
| |
Rignanese, Gian-Marco |
|
Hemming, Björn
in Cooperation with on an Cooperation-Score of 37%
Topics
Publications (5/5 displayed)
- 2020Surface modification of additively manufactured 18% nickel maraging steel by ultrasonic vibration-assisted ball burnishingcitations
- 2015Determination of wear volumes by chromatic confocal measurements during twin-disc tests with cast iron and steelcitations
- 2012Equipment for the calibration of squareness standardscitations
- 2009Hot rolling tests with steel bars and silicon nitride rollscitations
- 2006Transfer of surface texture from silicon nitride rolls to stainless steel wire in cold-rollingcitations
Places of action
Organizations | Location | People |
---|
article
Hot rolling tests with steel bars and silicon nitride rolls
Abstract
An experimental study was carried out to investigate the possibilities to use rolls made from Si<sub>3</sub>N<sub>4</sub>–TiN ceramic composite in hot rolling of steel. The results show that the wear of the ceramic material was lower than the wear of a reference cast iron. The results suggest that the Si<sub>3</sub>N<sub>4</sub>–TiN material is beneficial to use in a hot rolling process, on condition that the temperature of the work piece material is held sufficiently high.