People | Locations | Statistics |
---|---|---|
Naji, M. |
| |
Motta, Antonella |
| |
Aletan, Dirar |
| |
Mohamed, Tarek |
| |
Ertürk, Emre |
| |
Taccardi, Nicola |
| |
Kononenko, Denys |
| |
Petrov, R. H. | Madrid |
|
Alshaaer, Mazen | Brussels |
|
Bih, L. |
| |
Casati, R. |
| |
Muller, Hermance |
| |
Kočí, Jan | Prague |
|
Šuljagić, Marija |
| |
Kalteremidou, Kalliopi-Artemi | Brussels |
|
Azam, Siraj |
| |
Ospanova, Alyiya |
| |
Blanpain, Bart |
| |
Ali, M. A. |
| |
Popa, V. |
| |
Rančić, M. |
| |
Ollier, Nadège |
| |
Azevedo, Nuno Monteiro |
| |
Landes, Michael |
| |
Rignanese, Gian-Marco |
|
Williams, Geraint
Swansea University
in Cooperation with on an Cooperation-Score of 37%
Topics
Publications (9/9 displayed)
- 2021Intergranular and Pitting Corrosion in Sensitized and Unsensitized 20Cr-25Ni-Nb Austenitic Stainless Steel
- 2020The role of niobium carbides in the localised corrosion initiation of 20Cr-25Ni-Nb advanced gas-cooled reactor fuel claddingcitations
- 2020Towards a Physical Description of the Role of Germanium in Moderating Cathodic Activation of Magnesiumcitations
- 2020The effect of sodium hydroxide on niobium carbide precipitates in thermally sensitised 20Cr-25Ni-Nb austenitic stainless steelcitations
- 2017In situ imaging of corrosion processes in nuclear fuel claddingcitations
- 2017Self-piercing riveting-a review
- 2015In situ imaging of corrosion processes in nuclear fuel cladding
- 2014Latent Fingerprint Visualization using a Scanning Kelvin Probe in Conjunction with Vacuum Metal Depositioncitations
- 2014The effect of setting velocity on the static and fatigue strengths of self-piercing riveted joints for automotive applications
Places of action
Organizations | Location | People |
---|
article
The role of niobium carbides in the localised corrosion initiation of 20Cr-25Ni-Nb advanced gas-cooled reactor fuel cladding
Abstract
The role of niobium carbide (NbC) inclusions in directing the initiation of localised corrosion in sensitised 20Cr-25Ni-Nb stainless steel is investigated using a range of in-situ scanning techniques, allowing visualisation of corrosion behaviour over multiple length scales. Volta potential mapping shows NbC inclusions are up to 30 mV noble to the matrix, while chromium-depleted grain boundaries are up to 65 mV less noble. Corrosion initiation, shown by scanning vibrating electrode technique to comprise highly localised anode sites, is observed at grain boundaries, adjacent to the location of NbC inclusion clusters which remain unaffected by anodic dissolution of the surrounding matrix.