People | Locations | Statistics |
---|---|---|
Naji, M. |
| |
Motta, Antonella |
| |
Aletan, Dirar |
| |
Mohamed, Tarek |
| |
Ertürk, Emre |
| |
Taccardi, Nicola |
| |
Kononenko, Denys |
| |
Petrov, R. H. | Madrid |
|
Alshaaer, Mazen | Brussels |
|
Bih, L. |
| |
Casati, R. |
| |
Muller, Hermance |
| |
Kočí, Jan | Prague |
|
Šuljagić, Marija |
| |
Kalteremidou, Kalliopi-Artemi | Brussels |
|
Azam, Siraj |
| |
Ospanova, Alyiya |
| |
Blanpain, Bart |
| |
Ali, M. A. |
| |
Popa, V. |
| |
Rančić, M. |
| |
Ollier, Nadège |
| |
Azevedo, Nuno Monteiro |
| |
Landes, Michael |
| |
Rignanese, Gian-Marco |
|
Polido, Mario
in Cooperation with on an Cooperation-Score of 37%
Topics
Publications (7/7 displayed)
- 2022Improving Properties of an Experimental Universal Adhesive by Adding a Multifunctional Dendrimer (G-IEMA): Bond Strength and Nanoleakage Evaluationcitations
- 2022Wear of zirconia/leucite glass-ceramics composites: A chewing simulator studycitations
- 2020Dentin Bonding and SEM Analysis of a New Experimental Universal Adhesive System Containing a Dendrimercitations
- 2018Comparative tribological study of two prosthetic dental materials: Zirconia and Vita enamic
- 2018Comparative study of the wear of the pair human teeth/Vita Enamic (R) vs commonly used dental ceramics through chewing simulationcitations
- 2017Effect of bleaching teeth with hydrogen peroxide on the morphology, hydrophilicity, and mechanical and tribological properties of the enamelcitations
- 2011Diffuse Reflectance of Dental Materials After Staining: A Comparative Study
Places of action
Organizations | Location | People |
---|
article
Wear of zirconia/leucite glass-ceramics composites: A chewing simulator study
Abstract
Leucite and zirconia are commonly used in the production of prosthetic dental materials. Leucite presents attractive optical properties but low toughness and wear resistance, which limits its use. Zirconia has much higher toughness, but due to aesthetic reasons and ageing issues, needs to be glass veneered. Chipping of such veneer is usually responsible for the abnormal wear induced on the antagonist teeth. Leucite reinforced with 25% of nano-zirconia is a promising alternative to overcome these issues, allowing the production of dental restorations without veneer. This study aims to investigate if leucite-zirconia composites have suitable optical, mechanical and tribological properties to be used in dental restoration. Samples with different compositions of leucite and/or nano-zirconia were produced by unidirectional compression and characterized concerning density, surface morphology, roughness, hardness, toughness, and translucency. Wear tests were performed in a chewing simulator using human cusps as counterbodies. Tests were also performed in glazed zirconia for comparison. 25% ZrO2 leads to the lowest wear of the tribological pair among the studied systems, except 100% ZrO2. This can be attributed to the toughening effect of zirconia and reduced size of third body particles. Abrasion was the main wear mechanism observed in this pair. In addition, this was the composite that presented the highest translucency.