People | Locations | Statistics |
---|---|---|
Naji, M. |
| |
Motta, Antonella |
| |
Aletan, Dirar |
| |
Mohamed, Tarek |
| |
Ertürk, Emre |
| |
Taccardi, Nicola |
| |
Kononenko, Denys |
| |
Petrov, R. H. | Madrid |
|
Alshaaer, Mazen | Brussels |
|
Bih, L. |
| |
Casati, R. |
| |
Muller, Hermance |
| |
Kočí, Jan | Prague |
|
Šuljagić, Marija |
| |
Kalteremidou, Kalliopi-Artemi | Brussels |
|
Azam, Siraj |
| |
Ospanova, Alyiya |
| |
Blanpain, Bart |
| |
Ali, M. A. |
| |
Popa, V. |
| |
Rančić, M. |
| |
Ollier, Nadège |
| |
Azevedo, Nuno Monteiro |
| |
Landes, Michael |
| |
Rignanese, Gian-Marco |
|
Durand-Panteix, Olivier
in Cooperation with on an Cooperation-Score of 37%
Topics
Publications (3/3 displayed)
- 2022Synthesis of 0.94 Na0.5Bi0.5TiO3 – 0.06 BaTiO3 (NBT-6BT) lead-free piezoelectric powder suitable for aerosol deposition (AD)citations
- 2016Elaboration of lead-free Na0.5Bi0.5TiO3–BaTiO3 (NBT-BT) thick films by aerosol deposition method (ADM)citations
- 2015Dense and highly textured coatings obtained by aerosol deposition method from Ti3SiC2 powder: Comparison to a dense material sintered by Spark Plasma Sinteringcitations
Places of action
Organizations | Location | People |
---|
article
Elaboration of lead-free Na0.5Bi0.5TiO3–BaTiO3 (NBT-BT) thick films by aerosol deposition method (ADM)
Abstract
Thick and dense ceramic films of lead-free 0.94 Na 0.5 Bi 0.5 TiO 3 – 0.06 BaTiO 3 (NBT-BT) composition were elaborated by aerosol deposition method (ADM) at room temperature. A powder of suitable grain size was elaborated by solid state reaction. Using this powder, two samples were elaborated by ADM respectively on glass and metallic substrates, in order to check for microstructure and electrical properties. This process allowed obtaining a thick film (3.2 µm) with dense microstructure. Measurement of electrical properties revealed a lossy dielectric behavior indicating interfacial phenomena at the electrode – film interface. The measurement of the ferroelectric hysteresis cycle does not show any characteristics of a ferroelectric behavior, but corresponds well to the one of a lossy non-linear dielectric. The absence of ferroelectricity is probably due to the low grain size of the obtained thick film (130 nm). Further experiments are in progress in order to try to obtain ferroelectric properties.