People | Locations | Statistics |
---|---|---|
Naji, M. |
| |
Motta, Antonella |
| |
Aletan, Dirar |
| |
Mohamed, Tarek |
| |
Ertürk, Emre |
| |
Taccardi, Nicola |
| |
Kononenko, Denys |
| |
Petrov, R. H. | Madrid |
|
Alshaaer, Mazen | Brussels |
|
Bih, L. |
| |
Casati, R. |
| |
Muller, Hermance |
| |
Kočí, Jan | Prague |
|
Šuljagić, Marija |
| |
Kalteremidou, Kalliopi-Artemi | Brussels |
|
Azam, Siraj |
| |
Ospanova, Alyiya |
| |
Blanpain, Bart |
| |
Ali, M. A. |
| |
Popa, V. |
| |
Rančić, M. |
| |
Ollier, Nadège |
| |
Azevedo, Nuno Monteiro |
| |
Landes, Michael |
| |
Rignanese, Gian-Marco |
|
Schuler, Monika
in Cooperation with on an Cooperation-Score of 37%
Topics
Publications (4/4 displayed)
- 2017Effect of tempering time on the mechanical properties of P91 flux cored wire weld metalcitations
- 2014Creep investigation and simulation of CB2 joints using similar rutile CB2 flux-cored wirecitations
- 2014Properties of a creep resistant 9Cr-1.5Mo-1Co cast steel joint welded with a matching flux-cored wirecitations
- 2014Simulation of microstructure and modelling of mechanical properties of CB2 flux cored wires weld metal
Places of action
Organizations | Location | People |
---|
article
Effect of tempering time on the mechanical properties of P91 flux cored wire weld metal
Abstract
ASME Grade 91 is one of the main materials for heavy-wall pipes in thermal power plants. Matching flux cored wires for welding P91 have already been available for several years and become more and more popular as flux cored arc welding (FCAW) offers several technical and economic advantages. To achieve high toughness of the weld metal at ambient temperature, temperature and/or time of post-weld heat treatment (PWHT) can be increased. As the temperature has to be kept below the transformation temperature Ac1, the range of suitable temperature is very small. In this contribution, the effect of increased tempering time on the mechanical properties at ambient temperature and elevated temperatures is investigated and the influence on long-term properties is discussed. Longer PWHT increases toughness of all-weld metal. MatCalc simulations and scanning electron microscopy (SEM) investigations indicate a coarsening effect of precipitates without detrimental effect on long-term creep properties.