People | Locations | Statistics |
---|---|---|
Naji, M. |
| |
Motta, Antonella |
| |
Aletan, Dirar |
| |
Mohamed, Tarek |
| |
Ertürk, Emre |
| |
Taccardi, Nicola |
| |
Kononenko, Denys |
| |
Petrov, R. H. | Madrid |
|
Alshaaer, Mazen | Brussels |
|
Bih, L. |
| |
Casati, R. |
| |
Muller, Hermance |
| |
Kočí, Jan | Prague |
|
Šuljagić, Marija |
| |
Kalteremidou, Kalliopi-Artemi | Brussels |
|
Azam, Siraj |
| |
Ospanova, Alyiya |
| |
Blanpain, Bart |
| |
Ali, M. A. |
| |
Popa, V. |
| |
Rančić, M. |
| |
Ollier, Nadège |
| |
Azevedo, Nuno Monteiro |
| |
Landes, Michael |
| |
Rignanese, Gian-Marco |
|
Figueira, Joana
in Cooperation with on an Cooperation-Score of 37%
Topics
Publications (4/4 displayed)
- 2017Improved thermoelectric properties of nanocrystalline hydrogenated silicon thin films by post-deposition thermal annealingcitations
- 2017Optimization of Cuprous Oxides Thin Films to be used as Thermoelectric Touch Detectorscitations
- 2016V2O5 Thin Films for Flexible and High Sensitivity Transparent Temperature Sensorcitations
- 2015Hydrogenated nanocrystalline silicon thin films with promising thermoelectric propertiescitations
Places of action
Organizations | Location | People |
---|
article
Optimization of Cuprous Oxides Thin Films to be used as Thermoelectric Touch Detectors
Abstract
<p>The electronic and optical properties of p-type copper oxides (CO) strongly depend on the production technique as it influences the obtained phases: cuprous oxide (Cu2O) or cupric oxide (CuO), the most common ones. Cu films deposited by thermal evaporation have been annealed in air atmosphere, with temperature between 225 and 375 °C and time between 1 and 4 h. The resultant CO films have been studied to understand the influence of processing parameters in the thermoelectric, electrical, optical, morphological, and structural properties. Films with a Cu2O single phase are formed when annealing at 225 °C, while CuO single phase films can be obtained at 375 °C. In between, both phases are obtained in proportions that depend on the film thickness and annealing time. The positive sign of the Seebeck coefficient (S), measured at room temperature (RT), confirms the p-type behavior of both oxides, showing values up to 1.2 mV·°C(-1) and conductivity up to 2.9 (Ω·m)(-1). A simple detector using Cu2O have been fabricated and tested with fast finger touch events.</p>